With
its special property, the mental W. is suitable for the TIG welding
and the other electrode materials alike. To enforce the welding
power of W electrode by adding rare-earth oxide in the mental W.,
the property of W can be improved greatly , with better electrode
arc ,more stability of arc column, and less burning loss of electrode
. The usual rare-earth annexing agents include the following: cerium
oxide, thorium oxide, lanthana , zirconia and yttrium oxide ect.
The mental Th and W electrode |
The
mental TH and W electrode: add thorium anhydride in the mental W.
The advantages of TH and W electrode:
The lower power of electronic
The higher temperature of second crystallization
The better electro-conductive nature
The good property of mechanical cutting
|
|
Make |
Adulterant |
Doping amount |
Color marker |
WT10 |
ThO2 |
0.9-1.20% |
yellow |
WT20 |
ThO2 |
1.80-2.20% |
red |
WT30 |
ThO2 |
2.80-3.20% |
purple |
WT40 |
ThO2 |
3.80-4.20% |
orange |
The mental TH and W electrode: is a kind
of universally used material of W, with a far perfect property than
the pure W. and it is widely used in the DC welding. It is easily
handled and widely used in many company nowadays even if under the
overload current ,being regarded as one portion of high welding
quality.
During the using of Thoriated tungsten, the effect of electricity
saving is obvious, the argon amperage could be reduced 20-50%.And
because of the welding amperage is low, splat is difficult to see
during the welding, the head of Thoriated tungsten is also difficult
to become round, the time of using is more longer.
Keep good air condition and properly deal with the wasted welding
material.
|
|